Abstract

A Mongolian chalcopyrite flotation concentrate was leached using sodium hypochlorite adjusted to different pH using hydrochloric acid. It was found that using a starting pH of below 5.0 resulted in more efficient leaching. The extent of chalcopyrite leaching was determined by the concentration of sodium hypochlorite with > 40% dissolution being achieved. The residue after leaching was found to consist primarily of unreacted chalcopyrite which would be suitable for further leaching or smelting.

Document Type

Journal Article

Date of Publication

2018

Volume

19

Issue

45

Publication Title

Mongolian Journal of Chemistry

Publisher

Mongolian Academy of Sciences

School

School of Engineering

Funders

Alexander Mining plc

Creative Commons License

Creative Commons Attribution 4.0 License
This work is licensed under a Creative Commons Attribution 4.0 License.

Comments

Welham, N. J., Temuujin, J., & Setoudeh, N. (2018). Leaching of a Mongolian chalcopyrite concentrate. Mongolian Journal of Chemistry, 19(45), 1-4. https://doi.org/10.5564/mjc.v19i45.1082

First Page

1

Last Page

4

Share

 
COinS
 

Link to publisher version (DOI)

10.5564/mjc.v19i45.1082